During continuous batch processing of steel plates, the cutting quality of a fiber laser cutter may gradually decline over time. Here, we discuss common problems and their solutions when the machine operates under optimal parameter settings.

 

Lasers vs. Plasmas: Which Cutting Machine is Right for You?

 

1. Slag Adhesion After Prolonged Cutting

 

Problem: After extended operation, melted metal fails to eject from the kerf, leading to slag buildup. Possible causes include:

  • Optical path misalignment (dirty or misaligned lenses).
  • Inconsistent assist gas flow (pressure fluctuations or nozzle blockage).
  • Plate temperature rise due to heat accumulation.

 

Diagnosis: Compare the kerf width between normal and degraded cutting sections. If the width differs, the issue likely stems from lens contamination or focus position deviation.

 

Solution:

  • Clean and inspect the cutting head lenses in a dust-free environment.
  • Use a 20x microscope to examine the laser output head. Gently wipe contaminated optics with a dust-free swab and anhydrous alcohol.

 

Warning: Do not disassemble optical components without proper training or equipment.

 

2. Overburning During Long-Term Thick Plate Cutting

 

Problem:

 

When cutting thick plates at slow speeds, heat accumulates in the material, increasing plate temperature and causing overburning.

 

Diagnosis & Solutions:

 

(1) Nozzle Check: If the nozzle overheats or shows abnormalities, inspect internal lenses for contamination or damage.

(2) Red Light Test: Place white paper near the nozzle (tilted at an angle). If shadows appear in the red laser dot, the lenses are dirty.

(3) Microscope Inspection: In a cleanroom, examine the fiber output head and cutting head internals under a microscope for contamination or defects.

 

3. Additional Common Issues

 

A. Gradual Decline in Cutting Speed

 

Cause: Lens degradation, gas pressure drop, or mechanical wear.

 

Solution:

  • Recalibrate focus and gas settings.
  • Replace worn nozzles or lenses.

 

B. Inconsistent Cutting Depth

 

Cause: Uneven material surface, focus drift, or gas flow issues.

 

Solution:

  • Ensure plate flatness and adjust focus.
  • Verify gas purity and pressure stability.

 

Preventive Measures

 

  • Regular Maintenance: Clean lenses, check gas filters, and inspect nozzles daily.
  • Temperature Control: Allow cooling intervals for thick-plate jobs or use air/water cooling systems.
  • Parameter Optimization: Adjust power/speed ratios for prolonged operations.

 

By addressing these issues promptly, cutting quality and machine longevity can be maintained. For further technical support or maintenance guidance, contact our service team rayther@raytherlasercutter.com.

 